  pepperball china0.68 caliber pepperball taiwan0.5 caliber pepperball china0.68 caliber pepper ball Japan0.5 caliber pepper ball taiwan0.68inch Police practice peppe0.68inch Movie special effects0.5inch Police practice ball0.68 icaliber marker ball pepperball factory0.68inch pepperball factoryWholesale pepper ballsWholesale 0.68 inch pepper balWholesale 0.5 inch pepper ballWholesale 0.43 inch pepper balSafe Pepper Ball ManufacturingPE plastic ball chinaPlastic shell paintball0.68 caliber pepperball0.68 caliber pepper ball0.50 caliber pepper ball17.27mm pepperball0.5 caliber pepper ball0.43 caliber pepper ball0.68 caliber powder ballpepper ball newspepperball taiwan
Products Home > Products >  
 
 
Causes of stress cracking of PSU plastic pepper ball
 
 
 
Detail
 

Because of the high processing temperature of PSU plastic pepper ball, if the molded PSU plastic pepper ball is not annealed, it is easy to crack and deform during use, which affects the accuracy and service life. The solution to PSU stress cracking is mainly annealing.

The annealing method of PSU plastic pepper balls is mainly that the plastic blank balls after injection are immediately soaked in hot oil. Generally, the oil temperature is controlled at about 160 degrees for about 4 hours, so that the treated PSU plastic pepper balls have good toughness, high strength and long service life, and the most important thing is that they will not crack and deform.

 
Copyright © 2015 0.4 and 0.68 caliber pepperball, OC, PAVA and CS powder patented ALL RIGHTS RESERVED.