  pepperball china0.68 caliber pepperball taiwan0.5 caliber pepperball china0.68 caliber pepper ball Japan0.5 caliber pepper ball taiwan0.68inch Police practice peppe0.68inch Movie special effects0.5inch Police practice ball0.68 icaliber marker ball pepperball factory0.68inch pepperball factoryWholesale pepper ballsWholesale 0.68 inch pepper balWholesale 0.5 inch pepper ballWholesale 0.43 inch pepper balSafe Pepper Ball ManufacturingPE plastic ball chinaPlastic shell paintball0.68 caliber pepperball0.68 caliber pepper ball0.50 caliber pepper ball17.27mm pepperball0.5 caliber pepper ball0.43 caliber pepper ball0.68 caliber powder ballpepper ball newspepperball taiwan
Products Home > Products >  
 
 
Solution to crack of PA plastic pepper ball with poor toughness
 
 
 
Detail
 

PA plastic pepper balls will become low in strength and toughness due to the change of environment, and some of them will crack or break. The main reason for this defect is the influence of environment on materials. How to improve this defect is to adjust the humidity of materials according to experience.

Humidity control of PA plastic pepper balls and PA plastic hollow pepper balls is a common method to improve the toughness of PA plastic pepper balls. There are two kinds of humidity control processes: steam wet method and natural wet method. The steam wet method of PA plastic pepper balls has the advantage of high efficiency, which can basically reach the required strength in 5 hours, while the natural wet method takes about 10 days to complete. It is the most economical and practical method to improve the strength and toughness of PA plastic pepper balls and PA plastic hollow pepper balls by temperature regulation.

 
Copyright © 2015 0.4 and 0.68 caliber pepperball, OC, PAVA and CS powder patented ALL RIGHTS RESERVED.